In this work the performance of CaO-doped Ni/ZrO2 catalysts in ethanol steam reforming was studied. The addition of CaO did not affect the morphology or the crystalline structure of the support. On the contrary, Ni reducibility markedly increased. Moreover, the Lewis acidity of zirconia gradually decreased as the CaO content increased, thus inhibiting coke deposition and improving the carbon balance. The addition of a basic oxide helps to prevent some of the side reactions responsible for coke formation and deposition, that can gradually deactivate the catalyst.
Ni/ZrO2 catalysts in ethanol steam reforming: Inhibition of coke formation by CaO-doping
CRUCIANI, Giuseppe;
2014
Abstract
In this work the performance of CaO-doped Ni/ZrO2 catalysts in ethanol steam reforming was studied. The addition of CaO did not affect the morphology or the crystalline structure of the support. On the contrary, Ni reducibility markedly increased. Moreover, the Lewis acidity of zirconia gradually decreased as the CaO content increased, thus inhibiting coke deposition and improving the carbon balance. The addition of a basic oxide helps to prevent some of the side reactions responsible for coke formation and deposition, that can gradually deactivate the catalyst.File in questo prodotto:
Non ci sono file associati a questo prodotto.
I documenti in SFERA sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.